AWS E8018-C1 Kukwesha Simbi Yekupisa Kwakaderera Electrode W606Fe Kukwesha Kwesimbi Kwekunyorova Kwehydrogen Yakaderera ARC

Tsananguro pfupi:

W606Fe (AWS E8018-C1) ielectrode yesimbi inodziya zvishoma ine hupfu hwesimbi uye hydrogen potassium coating yakaderera


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Tembiricha YakadereraKushongedza SimbiElectrode

W606Fe                                                     

GB/T E5518-C1

AWS A5.5 E8018-C1

Tsananguro: W606Fe ielectrode yesimbi inodziya zvishoma ine upfu hwesimbi uye hydrogen potassium coating yakaderera. Inogona kushandiswa pakushongedza nzvimbo dzese neAC neDC. Simbi yakachengetwa ine simba rakanaka pa -60°C. 

Kushandiswa: Kunoshandiswa pakusondera simbi ine tembiricha yakaderera senge 2.5Ni.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Si

Ni

S

P

≤0. 12

≤1.25

≤0.80

2.00 ~ 2.75

≤0.020

≤0.025

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Kukosha kwemhedzisiro (J)

-60℃

Yakavimbiswa

≥540

≥440

≥17

≥27

 

Kupararira kwehydrogen musimbi yakachengetwa: ≤6.0mL/100g (nzira yeglycerin) kana ≤10mL/100g (nzira yemercury kana gas chromatography)

Kuongororwa kweX-ray: Giredhi I

 

Inokurudzirwa yemagetsi:

(mm)

Dhayamita yetsvimbo

3.2

4.0

5.0

(A)

Welding Current

90 ~ 120

140 ~ 180

180 ~ 210

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe pa350℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira.

 