AWS E7015-G Electrode Yekushongedza Simbi Yekupisa Kwakaderera W607 Rodhi Yekushongedza ...

Tsananguro pfupi:

W607 (AWS E7015-G) ielectrode yesimbi inodziya zvishoma ine hydrogen sodium coating yakaderera


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Electrode Yekushongedza Simbi Yekupisa Yakaderera

W607                                                     

GB/T E5015-G

AWS A5.5 E7015-G

 

Tsananguro: W607 ielectrode yesimbi inodziya zvishoma ine hydrogen sodium coating yakaderera. Shandisa DCEP (direct current electrode positive) uye inogona kusungirirwa munzvimbo dzese. Simbi yakachengetwa ine simba rakanaka pa -60°C.

Kushandiswa: Kunoshandiswa pakushongedza simbi ine tembiricha yakaderera senge 09MnD.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Si

Ni

S

P

≤0.08

≤1.65

≤0.60

0.50 ~ 2.50

≤0.020

≤0.025

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Kukosha kwemhedzisiro (J)

-60℃

Yakavimbiswa

≥490

≥390

≥22

≥27

 

Kupararira kwehydrogen musimbi yakachengetwa: ≤6.0mL/100g (nzira yeglycerin) kana ≤10mL/100g (nzira yemercury kana gas chromatography)

Kuongororwa kweX-ray: Giredhi I

 

Inokurudzirwa yemagetsi:

(mm)

Dhayamita yetsvimbo

2.0

2.5

3.2

4.0

5.0

(A)

Welding Current

40 ~ 70

60 ~ 90

100 ~ 120

140 ~ 170

170 ~ 200

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe pa350℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira;

3. Chikamu chakasungirirwa chinogona kupikiswa pakupisa kunenge 150°C chisati chasungirirwa kudzivirira kutsemuka.

 