AWS E2594-16 Welding Electrode, Tsvimbo dzeWelding, Zvekushandisa zveWelding

Tsananguro pfupi:

AF2594-16 (AWS E2594-16) ielectrode yesimbi isina tsvina ine nitrogen ine kabhoni shoma ine titanium-calcium coating.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Kushongedza Simbi Isina KusimbaElectrode

AF2594-16

AWS A5.4 E2594-16

Tsananguro: AF2594-16 ielectrode yesimbi isina tsvina ine nitrogen ine kabhoni yakaderera zvikuru ine titanium-calcium coating. Inogona kushandiswa kune ese ari maviri AC neDC. PRE (kupikisa pitting value equivalent value kana pitting index) ≥ 40, simbi yakachengetwa ine resistance yakanaka yekupisa. Nekuda kwehuwandu hwakaderera hwekabhoni uye huwandu hwakati hwemolybdenum nenitrogen, simbi yakachengetwa ine resistance yakanaka yekupikisa pitting corrosion uye stress corrosion cracking.

Mashandisirwo: Inonyanya kushandiswa pakusondera simbi isina tsvina yemhando imwe chete mumaindasitiri emafuta ekunze, gasi rechisikigo uye petrochemical, akadai se00Cr25Ni7Mo4N, nezvimwewo.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤1.00

24.0 ~ 27.0

8.0 ~ 10.5

3.5 ~ 4.5

0.20 ~ 0.30

≤0.75

≤0.030

≤0.040

 

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Kureba

%

Yakavimbiswa

≥760

≥15

 

Inokurudzirwa yemagetsi:

Dhayamita yetsvimbo

()mm)

2.5

3.2

4.0

5.0

Welding Current

()A)

50 ~80

80 ~ 120

120 ~ 150

150 ~ 200

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe chete pakupisa kwe250℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave tichiita basa rekugadziraelectrode yekunamiras, tsvimbo dzekunamirauyezvinodyiwa zveweldingkwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira simbi isina nguraelectrode yekunamiras, maelectrode esimbi yekuwedera nekabhoni, maelectrode ekuwedera neasina alloy, maelectrode ekuwedera neasina alloy, maelectrode ekuwedera neasina alloy, maelectrode ekuwedera neasina alloy, mawaya ekuwedera neasina alloy, waya dzekuwedera neasina alloy, waya dzesimbi dzisina alloy, waya dzakavharirwa negasi, waya dzekuwedera nearuminiyamu, welding yearc yakanyudzwa pasi. waya, waya dzekuwedera nealloy dzenickel & cobalt, waya dzekuwedera nebrass, waya dzekuwedera neTIG & MIG, maelectrode etungsten, maelectrode ekugouging nekabhoni, nezvimwe zvinhu zvekuwedera nezvinodyiwa.

 


  • Yakapfuura:
  • Zvinotevera: