AWS A5.4 E309Mo-15 Stainless Steel Electrode ine Yakaderera Hydrogen Sodium Coating, Welding tsvimbo

Tsanangudzo Pfupi

A317 (AWS E309Mo-15) isimbi isina tsvina electrode ine yakaderera hydrogen sodium coating.


Product Detail

Product Tags

Stainless Simbi WeldingElectrode

A317                                     

GB/T E309Mo-15

AWS A5.4 E309Mo-15

Tsanangudzo: A317 isimbi isina tsvina electrode ine yakaderera hydrogen sodium coating.Shandisa DCEP (yakananga ikozvino electrode yakanaka).Iyo ine ngura iri nani, kutsemuka, uye oxidation kuramba kupfuura A302 nekuti simbi yakaiswa ine molybdenum.

Chishandiso: Inoshandiswa kukwirisa mhando imwechete yesimbi isina tsvina, inoumbwa simbi ndiro uye dissimilar simbi inoshingirira kune sulfuric acid medium (sarufa ammonia) corrosion.

 

Kemikari yakagadzirwa nesimbi weld (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Mechanical zvimiro zve weld simbi:

Test chinhu

Kusimba simba

Mpa

Elongation

%

Guaranteed

≥550

≥25

 

Yazvino inokurudzirwa:

Tsvimbo dhayamita

(mm)

2.0

2.5

3.2

4.0

5.0

Welding Current

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Cherechedza:

Iyo electrode inofanira kubikwa kweawa imwe painotenderera 250 ℃ isati yaitwa welding.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Isu tanga tichiita mukugadzirawelding electrodes, welding tsvimbo,uyewelding zvinodyiwakweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira simbi isina tsvinawelding electrodes, carbon steel welding electrodes, low alloy welding electrodes, surfacing welding electrodes, nickel & cobalt alloy welding electrodes, mild steel & low alloy welding wires, stainless steel welding wires, gas-shielded flux cored wires, aluminium welding wires, submerged arc welding. .waya, nickel & cobalt alloy welding waya, ndarira welding waya, TIG & MIG welding waya, tungsten electrodes, carbon gouging electrodes, uye zvimwe welding accessories & consumables.

 


  • Zvakapfuura: