Tsvimbo yeWelding AWS A5.11 ENiCrFe-3 Nickel Based Alloy Welding Electrodes, Nickel Arc Welding Rods

Tsananguro pfupi:

Ni307-3 (AWS ENiCrFe-3) ielectrode yakagadzirwa ne nickel ine hydrogen sodium coating shoma. Shandisa DCEP (direct current electrode positive).


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Nickel uye Nickel Alloy Welding Electrode

Ni307-3                                                     

GB/T ENi6182

AWS A5.11 ENiCrFe-3

Tsananguro: Ni307-3 inikeliElectrode yakagadzirwa ne hydrogen sodium coating yakaderera. Shandisa DCEP (direct current electrode positive). Inodzivirira kupwanyika zvakanaka nekuti weld ine huwandu hwakati hwe manganese, niobium, nezvimwe zvinhu zvinosanganisa simbi.

Kushandiswa: Inoshandiswa pakushongedzanikeli-chromium-iron alloys (yakadai seUNS N06600) uye pamusoro pesimbi. Tembiricha yekushanda kazhinji haisi yepamusoro kupfuura 480 ° C, uye kuramba kutsemuka kwakanaka. Yakakodzera kumidziyo yeatomu yechoto uye kusanganisa tangi remakemikari.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Fe

P

S

Si

Cu

≤0.10

5.0 ~ 10.0

≤10.0

≤0.020

≤0.015

≤1.0

≤0.5

Ni

Ti

Mo

Nb

Ta

Zvimwe

 

≥60.0

≤1.0

13.0 ~ 17.0

1.0 ~ 3.5

≤0.30

≤0.50

 

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Yakavimbiswa

≥550

≥360

≥27

 

Inokurudzirwa yemagetsi:

Dhayamita yetsvimbo

(mm)

2.5

3.2

4.0

5.0

Welding current

(A)

60 ~ 90

80 ~ 100

110 ~ 150

130 ~ 180

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe chete pakupisa kwe300℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira. Edza kushandisa arc pfupi kunamira.

 


  • Yakapfuura:
  • Zvinotevera: