Tyue Brand Best Arc Welding Electrodes AWS ENiCrFe-1 Nickel Welding Rod, Chimuti Chekushongedza

Tsananguro pfupi:

Ni307-1 (AWS ENiCrFe-1) ielectrode yakagadzirwa ne nickel ine hydrogen sodium shoma. Shandisa DCEP (direct current electrode positive).


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Nickel uye Nickel Alloy Welding Electrode

Ni307-1                                                     

GB/T ENi6062

AWS A5.11 ENiCrFe-1

Tsananguro: Ni307-1 ielectrode yakagadzirwa nenickel ine hydrogen sodium shoma. Shandisa DCEP (direct current electrode positive). Sezvo weld ine Nb, simbi yakachengetwa ine plasticity yakanaka uye inodzivirira kutsemuka.

Mashandisirwo: Inoshandiswa pakusanganisa nickel-chromium-iron alloys (senge UNS N06600, UNS N06601) uye pamusoro pesimbi. Ine hunhu hwakanaka hwekusanganisa simbi. Inogona zvakare kushandiswa patembiricha yekushanda ye980°C, asi kana tembiricha yakakwira kupfuura 820°C, kuramba kweoxidation nesimba zvinodzikira.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Fe

Si

Cu

Ni

Cr

Nb + Ta

S

P

Zvimwe

≤0.08

≤3.5

≤11.0

≤0.8

≤0.5

≥62.0

13.0 ~ 17.0

0.5 ~ 4.0

≤0.015

≤0.020

≤0.50

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Yakavimbiswa

≥550

≥360

≥27

 

 

Inokurudzirwa yemagetsi:

Dhayamita yetsvimbo

(mm)

2.5

3.2

4.0

5.0

Welding current

(A)

60 ~ 90

80 ~ 110

110 ~ 150

130 ~ 180

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe chete pakupisa kwe300℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira. Edza kushandisa arc pfupi kunamira.

 

 


  • Yakapfuura:
  • Zvinotevera: