Waya Yekushongedza yeNickel Alloy ERNiCu-7 Nickel Tig Wire Filler Metal

Tsananguro pfupi:

ERNiCu-7 isimbi ye nickel-copper yakagadzirirwa kusanganisa Monel.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Nickel AlloyWaya yekunamiraWaya yeTigERNiCu-7

Maitiro
EN ISO 18274 - Ni 4060 - NiCu30Mn3Ti
AWS A5.14 – ER NiCu-7

 

Zvimiro uye Mashandisirwo

Chidimbu chenickel-copper chakagadzirirwa kusanganisa Monel.

Chitarisiko chakanaka chebeads uye inodzivirira ngura zvakanaka mu saline solutions.

Simbi yesimbi inonamira zvakanaka inodzivirira ngura dzakawanda.

Iyi alloy inoshandiswawo pakufukidza weld.

Inoshandiswa zvakanyanya mukuvaka gungwa, kunyanya mugungwa, muchina wekupisa, mapaipi, muzviteshi zvekubvisa munyu, mumakemikari, muindasitiri yepetrochemical uye muinjiniya yesimba nezvimwewo.

Zvinhu Zvakajairika Zvekushandisa

Monel alloys 400 uye 404*
* Rondedzero inotsanangura, kwete yakazara

 

 

Kuumbwa kweMakemikari %

C%

Mn%

Fe%

P%

S%

Si%

zvakanyanya

3.00

0.50

zvakanyanya

zvakanyanya

zvakanyanya

0.15

4.00

2.50

0.020

0.015

1.00

Cu%

Ni%

Co%

Ti%

Al%

Nb+Ta%

28.00

62.00

zvakanyanya

1.50

zvakanyanya

zvakanyanya

32.00

69.00

1.00

3.00

1.00

0.50

 

Zvivakwa zveMichina
Simba reKusimba ≥450 MPa
Simba reGoho ≥180 MPa
Kureba ≥30%
Simba reMhando ≥80 J

Hunhu hwemakanika hunofungidzirwa uye hunogona kusiyana zvichienderana nekupisa, gasi rekudzivirira, maparamita ekuwedera nezvimwe zvinhu.

 

Magasi ekudzivirira

TS EN ISO 14175 TIG: I1 (Argon)

 

Nzvimbo dzeWelding

TS EN ISO 6947 PA, PB, PC, PD, PE, PF, PG

 

Ruzivo rwekurongedza

Dhayamita

Kureba

Huremu

1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 kg

5 kg

5 kg

 

Mutoro: Kunyange hazvo paine zvese zvakaedzwa kuti pave nechokwadi chekuti ruzivo rwuripo rwakarurama, ruzivo urwu runogona kuchinja pasina chiziviso uye runogona kungoonekwa serwakakodzera kutungamirirwa nevanhu vose.