Waya Yekushongedza yeNickel Alloy ENiFe-Cl Mig Welding Wire

Tsananguro pfupi:

Waya yakasimba yeFerro-nickel inoshandiswa pakusanganisa simbi yakakandwa uye simbi yakapfava.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Nickel AlloyWaya yekunamiraENiFe-Cl

Zvimiro uye Mashandisirwo

Ferro-nikeliwaya yakasimba inoshandiswa pakusanganisa simbi yakakandwa uye simbi yakapfava.

Yakakodzera majoini akasiyana pakati pesimbi yakakandwa, simbi isina kusimba, simbi dzisina alloy shoma uye simbi dzisina ngura.

Zvinokurudzirwa pakusondera zvinhu zvakasanganiswa nesarufa yakawanda, phosphorus kana mafuta.

Ronda rakanyatsogadzirwa kuti rikwanise kupa waya zvakanaka.

Inowanzo shandiswa pakugadzirisa nekugadzira zvinhu zvakasiyana-siyana, kusanganisira kugadzirazve shafts, mavhiri, majoini akakosha pakati pesimbi nesimbi yakakandwa nezvimwewo.

Zvinhu Zvakajairika Zvekushandisa

Simbi yakakandwa yegrey, inonyungudika, ine maronda*
* Rondedzero inotsanangura, kwete yakazara

 

Maitiro
EN ISO 1071 – SC NiFe-1
AWS A5.15 - E NiFe-CI

 

Kuumbwa kweMakemikari %
C% Mn% Si% P% S%
zvakanyanya zvakanyanya zvakanyanya zvakanyanya zvakanyanya
2.00 0.80 0.20 0.03 0.03
Fe% Ni% Cu% Al%
rem. 54.00 zvakanyanya zvakanyanya
56.00 2.50 1.00

 

Zvivakwa zveMichina
Simba reKusimba 400 – 579 MPa
Simba reGoho -
Kureba -
Simba reMhando -

Hunhu hwemakanika hunofungidzirwa uye hunogona kusiyana zvichienderana nekupisa, gasi rekudzivirira, maparamita ekuwedera nezvimwe zvinhu.

 

Magasi ekudzivirira

EN ISO 14175 - I1, Ar + 1-2% O2

 

Nzvimbo dzeWelding

TS EN ISO 6947 PA, PB, PC, PD, PE, PF

 

Ruzivo rwekurongedza
Dhayamita
Huremu Spool NhumbiHuwandu
1.20 mm 15 kg BS300 72