Ni327-6 Nickel Alloy Welding Electrodes AWS A5.11 ENiCrMo-6 Welding Rods, Welding Structural Arc Welding Stick Electrodes

Tsananguro pfupi:

Ni327 -6 (AWS A5.11 ENiCrMo-6) ielectrode yakagadzirwa ne nickel ine hydrogen sodium coating shoma. Shandisa DCEP (direct current electrode positive).


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Nickel uye Nickel Alloy Welding Electrode

Ni327-6                                                     

GB/T ENi6620

AWS A5.11 ENiCrMo-6

Tsananguro: Ni327 -6 ielectrode yakavakirwa panickel ine hydrogen sodium coating shoma. Shandisa DCEP (electrode yakananga yemagetsi)yakanaka). Simbi yakachengetwa ine purasitiki yakanaka, kusimba uye kuramba kutsemuka. Simbi yakachengetwa ine chiyero chekuwedzera chakafanana nechesimbi, uye ine simba rakawanda uye kuramba ngura kwakasimba pakupisa kwemumba uye kupisa kwakanyanya.

Mashandisirwo: Inoshandiswa pakusanganisa simbi yeNi9%, uye inogona kushandiswawo pakusanganisa simbi dzakasiyana uye alloys dzakaoma kusanganisa.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Si

Ni

Mo

Fe

Cu

≤0.10

2.0 ~ 4.0

≤1.0

≥55.0

5.0 ~ 9.0

≤10.0

≤0.5

Nb + Ta

W

Cr

S

P

Zvimwe

 

0.5 ~ 2.0

1.0 ~ 2.0

12.0 ~ 17.0

≤0.015

≤0.020

≤0.5

 

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Yakavimbiswa

≥620

≥350

≥32

 

Inokurudzirwa yemagetsi:

Dhayamita yetsvimbo

(mm)

2.5

3.2

4.0

Welding current

(A)

50 ~ 70

80 ~ 100

110 ~ 150

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe chete pa300℃ isati yashandiswa pakusanganisa. Edza kushandisa arc pfupi kusanganisa;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira.

3. Edza kushandisa simba diki pakusanganisa, kusanganisa tambo dzakawanda uye kusanganisa tambo dzakawanda.

 

 