J607 (AWS E9015-D1) Maelectrode eSimbi Yekushongedza Akaderera Alloy Electrode yeSimbi Yakasimba Yepamusoro

Tsananguro pfupi:

J607 (AWS E9015-D1) ielectrode yesimbi ine simba rakawanda ine hydrogen sodium coating shoma.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Simbi Yechigadzirwa ChishomaKushongedzaElectrode

J607                                       

GB/T E6015-D1

AWS E9015-D1 

 

Tsananguro: J607 ielectrode yesimbi ine simba rakawanda ine hydrogen sodium coating shoma. Shandisa DCEP (direct current electrode positive), uye inogona kusungirirwa munzvimbo dzese.

Mashandisirwo: Inoshandiswa pakushongedza simbi yepakati nepakati ine kabhoni uye simbi ine simba rakaderera, senge Q420, nezvimwewo.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Si

Mo

S

P

≤0.12

1.25 ~ 1.75

≤0.60

0.25 ~ 0.45

≤0.035

≤0.035

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Kukosha kwemhedzisiro (J)

-30℃

Yakavimbiswa

≥590

≥490

≥15

≥27

Yakaedzwa

620 ~ 680

≥500

20 ~ 28

≥27

 

Kupararira kwehydrogen musimbi yakachengetwa: ≤4.0mL/100g (nzira yeglycerin) 

Kuongororwa kweX-ray: Giredhi I

 

Inokurudzirwa yemagetsi:

(mm)

Dhayamita yetsvimbo

2.0

2.5

3.2

4.0

5.0

5.8

(A)

KushongedzaZvazvino

60 ~ 80

70 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

210 ~ 260

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe pa350℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira;

3. Shandisa nzira pfupi yekupinza simbi pakusanganisa simbi. Nzira yakamanikana yekusanganisa simbi ndiyo yakakodzera.