D132 (B-83) Electrode Yekushongedza Yakagadzika, Tsvimbo Yekushongedza Yakaputirwa Pamusoro, Chimuti Chekushongedza Arc

Tsananguro pfupi:

Maelectrode ehydrogen mashoma ekushongedza patsva. Maweld anogona kugadzirwa nemashini (akatenderedzwa, akarongwa, akakuyiwa, nezvimwewo). Simba guru rekudzvanya. Anoramba zvakanaka kukweshwa zvine mwero.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Hardfacing Welding Stick ElectrodeRODO P

RODO PARA RECUBRIMIENTO MUDZIVIRI

Nhamba yeRudzi:B - 83

Kuongorora Simbi Yakachengetwa (Maitiro akajairika)

C

0.1%

Mn

0.9%

Si

0.8%

Cr

3.2%

 

Hunhu:

Maelectrode ehydrogen mashoma ekushongedza patsva. Maweld anogona kugadzirwa nemashini (akatenderedzwa, akarongwa, akakuyiwa, nezvimwewo). Simba guru rekudzvanya. Anoramba zvakanaka kukweshwa zvine mwero.

 

Zvimiro zveMichina:Kuomarara 27-31 HRc

 

Nzvimbo dzeKusonta:Yakati sandara, Yakati sandara, Pamusoro, Yakati sandara Mudenga.

 

Zvazvino uye Polarity:

Yekuchinjana kana yakananga magetsi

electrode kuenda kudanda rakanaka

ø mm

ø mukati

Amperage

3.20

1/8

110-130

4.00

5/32

140-180

5.00

2/16

190-240

 

Mashandisirwo: Muma feed roller, ma pulley, shangu dzemabhureki.

• Kuzadza matrakita

• Yakanaka kwazvo sehwaro hwekuputira kwakasimba pasimbi dzekabhoni.

kabhoni

• Zvigadziko, maekisero nemakonye efoshoro dzemakanika.

• Masirinda ekupwanya

• Marori ekutakura zvinhu

 

 

KUREBA: 350mm.

Huremu pabhokisi: 20 kg/44 lbs.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave tichiita basa rekugadziraelectrode yekunamiras, tsvimbo dzekunamira, uye zvinoshandiswa pakusonwa kwemidziyo kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira maelectrode esimbi isina ngura, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni & cobalt, mawaya esimbi yekabhoni & low alloy, waya dzesimbi yekabhoni & low alloy, waya dzesimbi yekabhoni, waya dzesimbi yekabhoni, waya dzakavharirwa negesi, waya dzesimbi yekabhoni ...

 

 

 

 


  • Yakapfuura:
  • Zvinotevera: