ER70S-2 Carbon Steel Welding Rods, Filler Metals yeGas Shielded Arc Welding Wire, Mutengesi Akanakisisa weSolder

Tsananguro pfupi:

ER70S2 iwaya yepamusoro yeMIG & TiG yekusanganisa simbi dzemhando dzese dzakapfava nedzakabhoni, ichigadzira simbi dzemhando yepamusoro dzisina maburi akawanda.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

ER70S2 iwaya yepamusoro yeMIG & TiG yekusanganisa simbi dzemhando dzese dzakapfava nedzakabhoni, ichigadzira simbi dzemhando yepamusoro dzisina maburi madiki. Iwaya ine mativi matatu (Zirconium, Titanium, uye Aluminium) inoita kuti ive sarudzo yakanaka yekusanganisa simbi pamusoro pengura nesimbi. Hapana flux inodiwa nechigadzirwa ichi.

ZVIMWE ZVINOSHANDISWA:

mapaipi nemidziyo yekuchera kuchera kunze kwenyika, basa resimbi yekuvaka

Nzvimbo yeWelding: F, V, OH, H Iye zvino: DCEP
Simba reKusimba, kpsi: 70
Simba reGoho, kpsi: 58
Kureba kwe 2”%: 22

Charpy V-Notch yakajairika: 35 ft.-lb. Pa -20 deg F

Kemikari yeWaya Yakajairika zvichienderana neAWS A5.18 (hunhu humwe chete ndihwo hwakanyanya)

C Mn Si P S Ni Cr Mo V Cu Ti Zr Al
0.07 0.90-1.40 0.40-0.70 0.025 0.035 0.15 0.15 0.15 0.03 0.50 0.05-0.15 0.02-0.12 0.05-0.15
Zvakajairika Zvekushongedza Zvimiro
Dhayamita Maitiro Volt Maampisi Gasi rekudzivirira
in (mm)
.035 (0.9) GMAW 28-32 165-200 Kupfuudza Spray 98% Argon+2% Okisijeni kana 75% Argon+25% CO2
.045 (1.2) GMAW 30-34 180-220 Kupfuudza Spray 98% Argon+2% Okisijeni kana 75% Argon+25% CO2
1/16 (1.6) GMAW 30-34 230-260 Kupfuudza Spray 98% Argon+2% Okisijeni kana 75% Argon+25% CO2
.035 (0.9) GMAW 22-25 100-140 Kutamiswa Kwemadenderedzwa Mapfupi 100% CO2 kana 75% Argon +25% CO2
.045 (1.14) GMAW 23-26 120-150 Kutamiswa Kwemadenderedzwa Mapfupi 100% CO2 kana 75% Argon +25% CO
1/16 (1.6) GMAW 23-26 160-200 Kutamiswa Kwemadenderedzwa Mapfupi 100% CO2 kana 75% Argon +25% CO
.035 (0.9) GTAW 13-16 60-100 100% Argon
.045 (1.14) GTAW 13-16 70-120 100% Argon
1/16 (1.6) GTAW 12-15 100-125 100% Argon
3/32 (2.4) GTAW 15-20 125-175 100% Argon
1/8 (3.2) GTAW 15-20 175-250 100% Argon