Waya yekuwedera yesimbi isina ngura inoshanda zvakanyanya, ine hunyanzvi hwekugadzira welding hwakanaka mukuwedera munzvimbo dzese. Inoshandiswa zvakanyanya mumaindasitiri: zvivakwa zvekuvaka, mota, mainjiniya emabhiriji, michina yekuchera migodhi, njanji, mapaipi emafuta, michina inotakura gasi, michina yemagetsi, nezvimwewo.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Kupatsanurwa kweAWS: AWS 5.9

TSANANGURO:

Waya yekuwedera yesimbi isina ngura inoshanda zvakanyanya, ine hunyanzvi hwekugadzira welding hwakanaka mukuwedera munzvimbo dzese. Inoshandiswa zvakanyanya muindasitiri: chimiro chekuvaka, mota, mainjiniya emabhiriji, michina yekuchera migodhi, njanji, mapaipi emafuta, michina inotakura gasi, michina yemagetsi, nezvimwewo.

Nhamba yemuenzaniso & Saizi:

1. Fekitori inopa OEM sevhisi.

2. Muenzaniso: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi nezvimwewo.

3. Saizi yewaya yeMIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4. Saizi yewaya yeTIG: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm .

NHANGANYAYA:

Tinopa mhando dzakasiyana dzewaya dzesimbi isina ngura, dzinosanganisira waya yeMig solid welding, waya yeTig rod welding uye waya ye submerged-arc welding, dzese dziri dzemhando yepamusoro uye dzinotengeswa pasi rese.

Kunze kwe308 ne309, tinopawo 304, 321, 347, 316L, 310, 2209, uye 201. Pamwe chete neruzivo rwakakosha rwakadai se318L, 904L, 2594, NiCrMo-3, Ni1.

Kurongedza:

Kurongedza waya yekuwedera neMig (paketi yedhiramu nespool)

Dhayamita: 0.8 - 2.0mm

Pakeji: 1 kg/spool, 5 kg/spool, 15 kg/spool, 20 kg/spool, 100 kg/drum, 200 kg/drum

Kurongedza waya yekuwedera netsvimbo yeTig rod (purasitiki chubhu)

Dhayamita: 1.0 - 5.0mm

Pakeji: 5 kg/pakeji

Waya yekuwedera yearc yakanyudzwa mumvura

Dhayamita: 2.5 - 5.0mm

Pakeji: 20kg/pakeji, 25 kg/pakeji

Kurongedza kusina kwakarerekera uye OEM zvinogamuchirwa!

ZVINHU ZVEKUGADZIRA WEWAYA YEKUWEDZERA SIMBIRI YAKASARA:

Nhamba yeModhero

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304L

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

ZVINHU ZVEWAYA YEKUWELDING:

Nhamba yeModhero

Simba rekusimba reRm(Mpa)

Simba remubereko Rel kana Rp0.2(Mpa)

Kureba

(%)

Nhamba yeModhero

Simba rekusimba reRm(Mpa)

Simba remubereko Rel kana Rp0.2(Mpa)

Kureba

(%)

304

550

--

25

ER309LSi

510

320

25

304L

510

--

25

ER316

510

320

25

ER307

590

350

25

ER316L

510

320

25

ER308

550

350

25

ER316LSi

510

320

20

ER308L

510

320

25

ER310

550

350

25

ER308LSi

510

320

25

ER347

550

350

25

ER309

550

350

25

ER317

550

350

25

ER309L

510

320

25

ER321

550

350

25

TIG neMIG simbi isina ngura yekuwedera waya yakagadzirwa

YB5092-2005

AWS

Kuumbwa kweMakemikari %

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307Si

0.075

0.78

6.7

0.022

0.01

19.8

8.8

H06Cr21Ni10

ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

ER308Si

0.045

0.85

1.5

0.022

0.01

20.8

9.8

H06Cr24Ni13

ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

H06Cr19Ni12Mo2

ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

ER316LSi

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

H07Cr20Ni34Mo2Cu3Nb

ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Nhamba 0.7

H02Cr20Ni34Mo2Cu3Nb

ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nhamba 0.35

H08Cr20Ni10Ti

ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

Ti9xC-1.0

H08Cr21 Ni10Nb

ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

Nb1xC-1.0

H12Cr26Ni21

ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

Cu 1.80

H03Cr22Ni9Mo3N

ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

Nhamba 0.08-0.20

H04Cr25Ni5Mo3Cu2N

ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

H03Cr24Ni13MoL

ER309L Mwedzi

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

Cu;3 Nb;0.28

H08Cr26Ni5Mo2

ER453s

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

H05Cr22Ni11Mn6Mo3VN

ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N;0.20 V;0.18