AWS ENiCu-7 Nickel Alloy Welding Rods Ni70Cu30 Nickel Based Welding Electrodes Manual Metal Arc Electrodes

Tsananguro pfupi:

Ni202 (AWS ENiCu-7) ielectrode yeNi70Cu30 Monel alloy ine titanium calcium coating. Inogona kushandiswa kune AC neDC.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Nickel uye Nickel Alloy Welding Electrode

Ni202                                                     

GB/T ENi4060

AWS A5.11 ENiCu-7

Tsananguro: Ni202 ielectrode yeNi70Cu30 Monel alloy ine titanium calcium coating. Inogona kushandiswa kune ese ari maviri AC neDC. Simbi yakachengetwa ine simba rakanaka rekudzivirira kupwanyika nekuda kwehuwandu hwakakodzera hwemanganese neniobium. Inoshanda zvakanaka pakuwelda uye ine arc combustion yakasimba, haina kupararira zvakanyanya, inobvisa tsvina zviri nyore, uye ine weld yakanaka.

Mashandisirwo: Inoshandiswa pakunamira nickel-copper alloy nesimbi dzakasiyana, uye inogonawo kushandiswa sechinhu chinochinjika.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Fe

Si

Nb

Al

Ti

Cu

Ni

S

P

≤0.15

≤4.0

≤2.5

≤1.5

≤2.5

≤1.0

≤1.0

27.0 ~ 34.0

≥62.0

≤0.015

≤0.020

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Yakavimbiswa

≥480

≥200

≥27

 

Inokurudzirwa yemagetsi:

Dhayamita yetsvimbo

(mm)

2.5

3.2

4.0

Welding current

(A)

50 ~ 80

90 ~ 110

110 ~ 150

 

Cherechedza:

1. Electrode inofanira kubikwa kweawa imwe chete pakupisa kwe250℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira.

 