AWS E10015-G Kusimba Kwakanyanya KweHydrogen Electrode Yakaderera Yepamusoro J707RH Tsinga Yekushongedza Yesimbi Yakaderera Yesimbi

Tsananguro pfupi:

J707RH (AWS E10015-G) ielectrode yehydrogen yakasimba zvikuru ine hydrogen sodium shoma.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Electrode Yesimbi Yekushongedza Yesimbi Yakaderera

J707RH                               

GB/T E7015-G

AWS E10015-G

 

Tsananguro: J707RH ielectrode yehydrogen yakasimba zvikuru ine hydrogen sodium shoma. Shandisa DCEP (direct current electrode positive) uye inogona kusungirirwa munzvimbo dzese. Mashandiro ekugadzirisa welding akanaka. Kukombama kunotonhora, kuramba kutsemuka uye kuramba kuputika kwemajoini akasungirirwa zvakanaka. Simbi yakachengetwa ine plasticity yakakura uye yakasimba.

Mashandisirwo: Inoshandiswa pakusanganisa zvivako zvehull, uye yakakodzerawo pakusanganisa zvivako zvakakosha zvesimbi yakasimba yeRp0.2≥590MPa.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Cr

Si

Ni

Mo

S

P

S + P

≤0.10

1.20 ~ 1.60

0.08 ~ 0.20

0.30 ~ 0.60

1.40 ~ 2.00

0.25 ~ 0.50

≤0.020

≤0.020

≤0.035

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Kukosha kwemhedzisiro (J)

-50℃

Yakavimbiswa

≥690

≥590

≥15

≥34

 

Kupararira kwehydrogen musimbi yakachengetwa: ≤4.1mL/100g (nzira ye mercury kana gas chromatography)

Kuongororwa kweX-ray: Giredhi I

 

Inokurudzirwa yemagetsi:

(mm)

Dhayamita yetsvimbo

4.0

5.0

(A)

Welding Current

160 ~ 180

180 ~ 220

 

Cherechedza:

1. Electrode inofanira kubikwa kwemaawa maviri pa400℃ isati yashandiswa pakunamira;

2. Zvakakosha kuchenesa ngura, mafuta, mvura, uye tsvina pazvikamu zvekunamira usati wanamira;

3. Shandisa nzira pfupi yekupinza simbi pakusanganisa simbi. Nzira yakamanikana yekusanganisa simbi ndiyo yakakodzera.

 