Mutengo weFekitori weWelding Rod/Welding Material Welding Electrode (Aws E6013)

Tsananguro pfupi:

J556 (AWS E8016-G) ielectrode yesimbi ine alloy yakaderera ine hydrogen potassium yakaderera. AC neDC zvese zvinogona kushandiswa, uye zvinogona kusungirirwa munzvimbo dzese.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Ita basa rakazara rekugutsa zvese zvinodiwa nevatengi vedu; kuwana kufambira mberi nguva dzose nekusimudzira kufambira mberi kwevatengi vedu; kukura kuva mubatsiri wekupedzisira wevatengi uye kuwedzera zvido zvevatengi veFactory Price Welding Rod/Welding Material Welding Electrode (Aws E6013), Tinogara tichibvumirana pakugadzira chigadzirwa chitsva chekugadzira kuti chigutse chikumbiro chevatengi vedu pasi rese. Tibatanei uye ngatiite kuti kutyaira kuve kwakachengeteka uye kunonakidza pamwe chete!
Ita basa rakazara rekugutsa zvese zvinodiwa nevatengi vedu; kuwana kufambira mberi nguva dzose nekusimudzira kufambira mberi kwevatengi vedu; kukura kuva mubatsiri wekupedzisira wevatengi uye kuwedzera zvido zvevatengi kuneChina Welding Electrode uye Welding Rod, Zvigadzirwa zvedu zvinotengeswa kunze kwenyika pasi rese. Vatengi vedu vanogara vachigutsikana nemhando yedu yakavimbika, masevhisi edu anotarisana nevatengi uye mitengo inokwikwidzana. Chinangwa chedu "ndechekuramba tichiwana kuvimbika kwenyu nekuzvipira kwedu mukuvandudza mhinduro dzedu nemasevhisi edu nguva dzose kuitira kuti tive nechokwadi chekuti vashandisi vedu, vatengi, vashandi, vatengesi pamwe nenharaunda dzepasi rose dzatinoshanda pamwe chete".
ZVINOSHANDISWA:

Kusonwa kwesimbi dze9% Cr-1% Mo uye 9% Cr - 2% Mo dzinoshandiswa pamagetsi nemidziyo ine simba rakawanda.

TSANANGURO:

PA-8016-B8 ielectrode ine hydrogen shoma ine simbi ye weld ine 9%Cr-1%Mo. Yakagadzirirwa simbi nesimbi dzinopisa zvakanyanya dzebasa re hydrogen inopisa, kunyanya muindasitiri ye petrochemical. Electrode iyi inogona kutenderwa nekuda kwesimba rayo rekusimba, kusimba kwayo uye kuramba kupisa kwakanyanya.

ZVINOKOSHA PAMUSORO PEKUSHANDISA:

1. Omesai maerekitirodhi pa350-400°C kweinenge awa imwe chete musati mashandisa uye chengetai maerekitirodhi pa100-150°C mushure mekuaomesa muchingwarira kuchengetedza hunyoro.

2. Shandisa nzira yekudzokera shure kana kurovera arc paplate diki yesimbi yakagadzirirwa chinangwa ichi kudzivirira maburi ekuputira paarc kutanga.

3. Chengeta denderedzwa riri pfupi sezvinobvira.

4. Pisa pa100-150°C. Tembiricha inoshandiswa inosiyana zvichienderana neukobvu hweplate uye rudzi rwesimbi inofanira kusungirirwa.

5. Chenjerera kuti usapfuure mwero wakakodzera wekupisa nekuti mwero wakawandisa wekupisa unokonzera kuora kwesimba remagetsi uye simba resimbi yesimbi ye weld.

IV. KUUMBIKA KWEMAKEMIKIRI AKAJAIWA ESIMBI YEWELD (%):

C

Si

Mn

Cr

Mo

0.06

0.42

0.68

9.38

1.05

V. ZVINHU ZVEMAKANIKISI ZVEWELD STEAL ZVAKAJAIRWA:

Simba reKusimba N/mm2(Ksi)

Nzvimbo yeGoho N/mm2

(Ksi)

Kureba %

PWHT

705 (102)

560 (81)

24

740°C x awa imwe chete

VI. ZVINHU ZVEKUWEDZERA: ZVINHU ZVOSE

VII. SAIZI UYE ZVINHU ZVINOKURUDZIRWA (AC/DC+):

Dhayamita (mm)

2.5

3.2

4.0

5.0

Kureba (mm)

350

350

400

400

Ampere

Furati

55 - 85

90 - 130

130 - 180

180 - 240

V & OH

50 - 80

80 - 115

110 - 170

150 - 200

Ita basa rakazara rekugutsa zvese zvinodiwa nevatengi vedu; kuwana kufambira mberi nguva dzose nekusimudzira kufambira mberi kwevatengi vedu; kukura kuva mubatsiri wekupedzisira wevatengi uye kuwedzera zvido zvevatengi veFactory Price Welding Rod/Welding Material Welding Electrode (Aws E6013), Tinogara tichibvumirana pakugadzira chigadzirwa chitsva chekugadzira kuti chigutse chikumbiro chevatengi vedu pasi rese. Tibatanei uye ngatiite kuti kutyaira kuve kwakachengeteka uye kunonakidza pamwe chete!
Mutengo weFekitoriChina Welding Electrode uye Welding Rod, Zvigadzirwa zvedu zvinotengeswa kunze kwenyika pasi rese. Vatengi vedu vanogara vachigutsikana nemhando yedu yakavimbika, masevhisi edu anotarisana nevatengi uye mitengo inokwikwidzana. Chinangwa chedu "ndechekuramba tichiwana kuvimbika kwenyu nekuzvipira kwedu mukuvandudza mhinduro dzedu nemasevhisi edu nguva dzose kuitira kuti tive nechokwadi chekuti vashandisi vedu, vatengi, vashandi, vatengesi pamwe nenharaunda dzepasi rose dzatinoshanda pamwe chete".