Waya yeTig neMig A5.28 ER80S-D2, Simbi Yekuzadza Simbi Isina Chiyero Chekushongedza Arc Yakadzivirirwa neGasi

Tsananguro pfupi:

ER80S-D2 iwaya yakasimba yesimbi isina kusimba inoshandiswa mumamiriro ezvinhu apo porosity iri dambudziko kana paunofanira kurwisa huwandu hwakawanda hwesarufa kana kabhoni musimbi yako.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

A5.28 ER80S-D2, Simbi Yekuzadza Simbi Isina Chiyero Chekushongedza Arc Yakachengetedzwa Negesi

ER80S-D2 iwaya yakasimba yesimbi isina kusimba inoshandiswa mumamiriro ezvinhu apo porosity iri dambudziko kana paunofanira kurwisa huwandu hwakawanda hwesarufa kana kabhoni musimbi yako. Ine huwandu hwakawanda hwemanganese nesilicon kuti ipe kunyorova kwakanaka pamwe nekutsungirira ngura nekukasira.

Mashandisirwo Akajairika: mashandisirwo emhando ye x-ray, ma welds ane simba guru, ma boiler esteam, matangi ekumanikidza, mapaipi egasi, kuchinjana kwekupisa, indasitiri ye petrochemical

Kirasi yeAWS: ER80S-D2 Chitupa: AWS A5.28/A5.28M:2005
Chiwanikwa: ER80S-D2 AWS/ASME SFA A5.28

 

Nzvimbo yeWelding: F, V, OH, H Zvazvino:
GMAW-DCEP

 

Simba reKusimba, kpsi: Maminetsi makumi masere
Simba reGoho, kpsi: Maminetsi makumi matanhatu nemasere
Kureba %: 17 mamineti

Kemikari yeWaya Yakajairika zvichienderana neAWS A5.28 (hunhu humwe chete ndihwo hwakanyanya)

C Mn Si P S Ni Mo Cu Zvimwe
0.07-0.12 1.60-2.10 0.50-0.80 0.025 0.025 0.15 0.40-0.60 0.50 0.50
Zvakajairika Zvekushongedza Zvimiro
Dhayamita Maitiro Volt Maampisi Gasi rekudzivirira
in (mm)
.035 (0.9) GMAW 28-32 165-200 Kupfuudza 98% Argon/2% Okisijeni
.045 (1.2) GMAW 30-34 180-220 Kupfuudza 98% Argon/2% Okisijeni
1/16 (1.6) GMAW 30-34 230-260 Kupfuudza 98% Argon/2% Okisijeni
.035 (0.9) GMAW 22-25 100-140 Kutamiswa Kwemadenderedzwa Mapfupi 90% Helium/ 75% Argon / 25% CO2
.045 (1.2) GMAW 23-26 120-150 Kutamiswa Kwemadenderedzwa Mapfupi 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) GMAW 23-26 160-200 Kutamiswa Kwemadenderedzwa Mapfupi 90% Helium/ 75% Argon / 25% CO2
1/16 (1.6) GTAW 12-15 100-125 100% Argon
3/32 (2.4) GTAW 15-20 125-175 100% Argon
1/8 (3.2) GTAW 15-20 175-250 100% Argon

 