A5.13 ECoCr-C Cobalt Alloy Hardfacing Welding Rods Welding Inodzivirira Kupfeka Electrode Arc Welding Stick

Tsananguro pfupi:

A5.13 ECoCr-C Cobalt Alloy Hardfacing Welding Rods inoshandiswa pakuisa misoro yemavharuvhu, ma seal rings epombi ine pressure yakakwira uye zvikamu zvemacrusher.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

 

AWS Speicication:AWS A5.13/AME A5.13 ECoCr-C
ZVINOSHANDISWA:

Kuisa pamusoro pemisoro yemavharuvhu, mhete dzekusimbisa dzakagadzirwa nepombi ine simba rakawanda uye zvikamu zvemacrusher.
TSANANGURO:

COBALTARD 1FC covered electrode ndiyo yakanyanya kuomarara muboka re cobalt alloys inoshandiswa pakuora kwakanyanya pakupisa. Madhayi e alloy iyi ane huwandu hwakawanda hwe chromium carbides inokanganisa kuramba kupisa kwakanyanya. Kuwedzerwa kwe tungsten kunowedzera kuomarara pakupisa kwakanyanya uye kusimba kwe matrix kuti inamire zvakanaka uye irambe yakasimba pakuora. Inobatanidza zvakanaka nesimbi dzese, kusanganisira stainless steel.
ZVINOKOSHA PAMUSORO PEKUSHANDISA:

Pisa pa300ºC zvichikwira. Shandisa PHILARC temperature indicating sticks kana PHILARC interpass temperature gauge kuti uone kana tembiricha yakakodzera yawanikwa usati waisa welding. Kuti uwane rumwe ruzivo ona PHILARC Chart 4 Easy Steps yekuisa welding.

Zvinoshanda kupisa pa600ºC uye kutonhora zvishoma nezvishoma mushure mekunamira kuti zvisatsemuke.

Omesai maerekitirodhi pa 150-200ºC kwemaminitsi 30 - 60 musati mashandisa. Shandisai maovheni ekuomesa anotakurika ePHILARC.

KUOMA KWESTEAL DEPOSIT YEWELD: 50 – 56 HRC (520- 620 Hv)
KUUMBIKA KWEMAKEMIKIRI AKAJAIWA EWELD STAR (%):

C Si Mn Cr W Co
2.15 0.47 1.03 31.25 12.72 Bhari

Saizi dziripo uye dzinokurudzirwa (DC +):

Saizi (dhayamita mm) 3.2 4.0 5.0
Kureba (mm) 350 350 350
Range Yazvino (Amp) 90 - 120 110 - 150 140 - 180

 

 