AWS/ASME A 5.3 E 3003 Aluminium Welding Electrodes

Tsananguro pfupi:

Kubatanidza maaruminiyamu akasiyana-siyana uye kushandiswa mumvura yegungwa, aruminiyamu dzakasanganiswa nemanganese nemagnesium.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Bhodhi repadivi rakaderera rine madhirowa mana, akagadzirwa neruvara ruchena rine furemu yegoridhe inopenya uye magadzirirwo, uye girazi rakajeka rinofukidza pamusoro. Chinhu chakagadzirwa zvakanaka kune chero imba yekugara. Chakanakira chero ani zvake anoyemura fenicha ine magadzirirwo akanaka uye epamusoro.

Gillmore Alberto Collection yakanakira vagadziri vedzimba dzemhando yepamusoro nedzezviratidzwa.

Nemitsetse yakachena yemazuva ano uye zvinhu zvakapfava uye zvine hungwaru, chidimbu chimwe nechimwe (chinowanzoonekwa) sechinhu chepamusoro-soro chemukati membatya, chakagadzirwa nepfungwa dzekushanda. Zvishongo zvese zvemakesi ane lacquer zvinowanikwa muchena we satin matt kana grey matt, nesimbi yakanaka inopenya nebrass kana black chrome kuti iratidze chitarisiko chemazuva ano chinokwezva pasi rose.

Chimwe chezvinhu zvakasiyana muunganidzwa uyu igirazi rine ruvara rwakafanana nemakabati edu ese eAlberto kuti rigare kwenguva refu uye risingakanganisike. Uyezve, kune nzira dzakawanda dzekuchengetera zvinhu, sezvo mayuniti acho ari emhando yepamusoro uye anounzwa muzvikamu zvehukuru hunoshanda kuti aderedze kushushikana kunouya nekutakura nekuisa.


DIN: 1732: EL Si-Al Mn

ZVINHU & ZVINOSHANDISWA:

Pakushongedza arc, maaruminiyamu akasanganiswa nemanganese nemagnesium. Akanakirawo kubatanidza mhando dzakasiyana dzearuminiyamu uye kushandiswa mumvura yegungwa.

Electrode yekuwachisa arc yearuminiyamu ine slag yekusimudza yega yega. Mamwe magiredhi earuminiyamu akadai se12%Si, 5%Si uye E 1100, nezvimwewo anowanikwawo.

Siragi yekuzvisimudza yakasiyana.

Chipfeko chepurasitiki chena chakachena chinogara kwenguva refu chinopfuura zvigadzirwa zvemazuva ose kana chichidzivirira hunyoro.

Inogona kugadzirwa mumhando dzakasiyana-siyana dzemavara.

Inowanikwa mumagaba ePURE ALUMINUM ekudhonza akavharwa zvakanaka kana mumabhegi efoil akavharwa ne vacuum kuti igare kwenguva refu.

ONGORORO YESITAMBO YEKUWEDZERA (HUREMU HWAKANAKA %):

Ruvara rweFlux: Ruchena kana Ruvara Rwakagadzirwa

Si Cu Fe Zn Mn Be Zr Ti Al
0.14 .07 0.23 .002 1.3 .0001 .0004 .009 Bhari.

ZVINHU ZVEMAKANIKISI ZVAJAIWA:

Simbi Yakasungirirwa Isina Kusanganiswa Kukosha Kusvika ku

Simba reKusimba 34,000 psi (250 N/MPa)

Simba reKubereka 20,000 psi (150 N/MPa)

Kureba 10%

ZVINOITWA NEKUWELDING ZVIRIPO & MIRAYIRO:

Zvinokurudzirwa Kushandiswa Kwemagetsi: DC Reverse (+)
Dhayamita (mm) 3/32 (2.5) 1/8 (3.25)
Amperage shoma 50 70
Amperage yepamusoro 80 120

Matekiniki Ekushongedza: Tanga nekushandisa chikamu chepamusoro che amperage range. Isa electrode nekukurumidza uye famba nekukurumidza uchichengetedza arc gap iri pedyo.

Nzvimbo dzeWelding: Flat, Yakatsetseka

MARI YEKUDZORA PACHIKAMU:

Dhayamita (mm) Kureba (mm) Simbi yeWeld/Electrode Electrodesper lb (kg) yesimbi yeWeld Nguva yeArc yeDepositionmin/lb (kg) Zvigadziriso zveAmperage Mwero weKupora
3/32 (2.5) 14″ (350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14″ (350) .23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14″ (350) .33oz (9.6g) 48 (107) 47 (103) 135 90%

ZVINOFANIRA KUPAKISWA KWEMA ELECTRODE & ZVIKAMU:

Dhayamita (mm) 3/32 (2.5) 1/8 (3.25) 5/32 (4.0)
Kureba (mm) 14″ (350) 14″ (350) 14″ (350)
Maerekitirodhi / lb 49 33 23
Maerekitirodhi / kg 108 73 51