Maelectrode eAluminium Welding eAWS/ASME A 5.3 E1100 eAluminium AWS/ASME A5.3 E1100

Tsananguro pfupi:

Pakushongedza arc, maaruminiyamu akasanganiswa nemhangura, silicon, uye magnesium. Yakanakirawo kubatanidza mhando dzakasiyana dzearuminiyamu.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Aruminiyamu neAruminiyamu Chiwanikwa Electrode

L109

GB/T E1100

AWS A5.3 E1100

Tsananguro: L109 ielectrode yearuminiyamu yakachena ine pendi yakagadzirwa nemunyu. Shandisa DCEP (electrode yemagetsi yakananga). Edza kushandisa arc pfupi kusanganisa.

Kushandiswa: Kunoshandiswa pakunamira mapurasitiki earuminiyamu nemidziyo yearuminiyamu yakachena.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

Si+Fe

Cu

Mn

Zn

Al

Zvimwe

≤0.95

0.05 ~ 0.20

≤0.05

≤0.10

≥99.0

≤0.15

 

 

Hunhu hwesimbi ye weld:

Chinhu chekuyedza

Simba rekusimba

Mpa

Yakavimbiswa

≥80

 

Inokurudzirwa yemagetsi:

Dhayamita yetsvimbo

()mm)

3.2

4.0

5.0

Welding current

()A)

80 ~ 100

110 ~ 150

150 ~ 200

 

Cherechedza:

1. Electrode iri nyore kukanganiswa nehunyoro, saka inofanira kuchengetwa mumudziyo wakaoma usingapindi mhepo kuti isaora nekuda kwehunyoro; electrode inofanira kubikwa pa150°C kweawa imwe kusvika maviri isati yaiswa welding;

2. Maplate ekumashure anofanira kushandiswa usati wabatanidza, uye kusanganisa kunofanira kuitwa mushure mekudziya kusvika 200 ~ 300°C zvichienderana neukobvu hwekubatanidza; tsvimbo yekusanganisa inofanira kunge yakatarisana nepamusoro pekubatanidza, arc inofanira kunge iri pfupi sezvinobvira, uye kutsiva tsvimbo dzekusanganisa kunofanira kuitwa nekukurumidza;

3. Kubatanidza kunofanira kucheneswa kubva mumafuta netsvina isati yabatanidzwa, uye tsvina inofanira kubviswa nokungwarira mushure mekusanganisa, uye kusukurudzwa neutsi kana mvura inopisa.

 

 

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave tichigadzira maerekitironi ekuwelda, tsvimbo dzekuwelda, uye zvinhu zvinoshandiswa pakuwelda kweanopfuura makore makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira maelectrode esimbi isina ngura, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni, maelectrode esimbi yekabhoni & cobalt, mawaya esimbi yekabhoni & low alloy, waya dzesimbi yekabhoni & low alloy, waya dzesimbi yekabhoni, waya dzesimbi yekabhoni, waya dzakavharirwa negesi, waya dzesimbi yekabhoni ...

 

EN 573-3: E Al

DIN: 1732: EL-Al

ZVINHU & ZVINOSHANDISWA:

Pakushongedza arc, maaruminiyamu akasanganiswa nemhangura, silicon, uye magnesium. Yakanakirawo kubatanidza mhando dzakasiyana dzearuminiyamu.

Electrode yearuminiyamu yakachena ine slag inosimudza yega. Mamwe magiredhi earuminiyamu akadai se12%Si, 5%Si uye Al Mn, nezvimwewo anowanikwawo.

Siragi yekuzvisimudza yakasiyana.

Chipfeko chepurasitiki chena chakachena chinogara kwenguva refu chinopfuura zvigadzirwa zvemazuva ose kana chichidzivirira hunyoro.

Inogona kugadzirwa mumhando dzakasiyana-siyana dzemavara.

Inowanikwa mumagaba ePURE ALUMINUM ekudhonza akavharwa zvakanaka kana mumabhegi efoil akavharwa ne vacuum kuti igare kwenguva refu.

Kuongororwa Kwesimbi Yese Yakasungirirwa (Huremu Hwakajairika%):

Ruvara rwakanaka: Chena kana Ruvara Rwakagadzirwa

Si Cu Fe Ti Mn Zn Be Al
.091 .05 .45 .01 .005 .002 .0002 Bhari.

ZVINHU ZVEMAKANIKISI ZVAJAIWA:

Simbi Yakasungirirwa Isina Kusanganiswa Kukosha Kwayo Kusvika ku:

Simba reKubata: 34,000 psi (250 N/MPa)

Simba reKubereka: 20,000 psi (150 N/MPa)

Kureba: 5%

Kushongedza Kwemazuva Ano & Mirayiridzo
Zvinokurudzirwa Kushandiswa Kwemagetsi: DC Reverse (+)
Dhayamita (mm) 3/32 (2.5) 1/8 (3.25)
Amperage shoma 50 70
Amperage yepamusoro 80 120

Matekiniki Ekushongedza: Tanga nekushandisa chikamu chepamusoro che amperage range. Isa electrode nekukurumidza uye famba nekukurumidza uchichengetedza arc gap iri pedyo.

Nzvimbo dzeWelding: Flat, Yakatsetseka

MARI YEKUDZORA PACHIKAMU:

Dhayamita (mm) Kureba (mm) Simbi yeWeld/Electrode Maerekitirodhi perlb (kg) esimbi yeWeld Nguva yeArc yeDeposition min/lb (kg) Zvigadziriso zveAmperage Mwero weKupora
3/32 (2.5) 14″ (350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14″ (350) .23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14″ (350) .33oz (9.6g) 48 (107) 47 (103) 135 90%

ZVINOFANIRA KUPAKISWA KWEMA ELECTRODE & ZVIKAMU:

Dhayamita (mm) 3/32 (2.5) 1/8 (3.25) 5/32 (4.0)
Kureba (mm) 14″ (350) 14″ (350) 14″ (350)
Maerekitirodhi / lb 49 33 23
Maerekitirodhi / kg 108 73 51

  • Yakapfuura:
  • Zvinotevera: