AWS/ASME 5.3 E 4047 Aluminium Welding Electrodes Aluminium Welding Rods Arc Welding Stick Supplier

Tsananguro pfupi:

Kune arc welding aruminiyamu dzakasanganiswa nemhangura, silicon, uye magnesium


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

EN 573-3: E AlSi12

DIN 1732: EL-Al Si12

ZVINHU & ZVINOSHANDISWA:

Pakushongedza arc, maaruminiyamu akagadzirwa nemhangura, silicon, uye magnesium.

Zvakare zvakanaka pakubatanidza mhando dzakasiyana dzealuminium.

12% Silicon aruminiyamu arc welding electrode ine slag yakasarudzika inosimudza yega. Mamwe marudzi earuminiyamu akadai seAl 99, Al Mn, nezvimwewo anowanikwawo.

Siragi yekuzvisimudza yakasiyana.

Chipfeko chepurasitiki chena chakachena chinogara kwenguva refu chinopfuura zvigadzirwa zvemazuva ose kana chichidzivirira hunyoro.
Inogona kugadzirwa mumhando dzakasiyana-siyana dzemavara.

Inowanikwa mumagaba ePURE ALUMINUM ekudhonza akavharwa zvakanaka kana mumabhegi efoil akavharwa ne vacuum kuti igare kwenguva refu.

Inowanikwawo muchimiro cheTIG sekodhi yechinhu 6047, muchimiro cheMIG sekodhi yechinhu 7091 uye sechisina chinhu.

Chishandiso cheTorch Brazing Alloy seItem Code 2191:

Kuongororwa Kwesimbi Yese Yakasungirirwa (Huremu Hwakajairika%)
Ruvara rweFlux: Ruchena kana Ruvara Rwakagadzirwa
12.1 .001 .15 .01 .003 .001
Si Cu Fe Mg Mn Zn
Kushongedza Kwemazuva Ano & Mirayiridzo
Zvinokurudzirwa Kushandiswa Kwemagetsi: DC Reverse (+)
Dhayamita (mm) 3/32 (2.5) 1/8 (3.25)
Amperage shoma 50 70
Amperage yepamusoro 80 120

Matekiniki Ekushongedza: Tanga nekushandisa chikamu chepamusoro che amperage range. Isa electrode nekukurumidza uye famba nekukurumidza uchichengetedza arc gap iri pedyo.
Nzvimbo dzeWelding: Flat, Yakatsetseka

MARI YEKUDZORA PACHIKAMU:

Dhayamita (mm) Kureba (mm) Simbi yeWeld/Electrode Maerekitirodhi pa lb (kg) yeWeldmetal Nguva yeArc yeKuisa pasi min/lb (kg) Zvirongwa zveAmperage Mwero weKupora
3/32 (2.5) 14″ (350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14″ (350) .23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14″ (350) .33oz (9.6g) 48 (107) 47 (103) 135 90%

ZVINOFANIRA KUPAKISWA KWEMA ELECTRODE & ZVIKAMU:

3/32 (2.5) 1/8 (3.25)
Kureba (mm) 14″ (350) 14″ (350)
Maerekitirodhi / lb 49 33
Maerekitirodhi / kg 108 73

  • Yakapfuura:
  • Zvinotevera: