AWS E8010-G Low Alloy Steel Welding Electrode, Mutengesi Akanakisisa weZvinhu Zvekushongedza

Tsananguro pfupi:

J555G (AWS E8010-G) ielectrode yakadzika yakatwasuka ine cellulose yakawanda sodium-coated.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Electrode Yesimbi Yekushongedza Yesimbi Yakaderera

J555G                                               

GB/T E5510-G

AWS A5.5 E8010-G

Tsananguro: J555G ielectrode yakadzika ine sodium yakawanda yakaputirwa ne cellulose. Shandisa DCEP (electrode yakananga yemagetsi). Yakakodzera kusungirirwa kwese kwese kwese kwese kwese kwese kwese kwese kwese kwese kwese kwese panzvimbo yepombi. Inogona kusungirirwa kune rumwe rutivi uye kugadzirwa kumativi ese, uye kumhanya kwekubatanidza kunokurumidza.

Kushandiswa: Kunoshandiswa pakushongedza mapaipi akasiyana-siyana esimbi asina kusimba.

 

Kuumbwa kwemakemikari esimbi ye weld (%):

C

Mn

Si

S

P

≤0.20

≥1.00

≤0.50

≤0.035

≤0.035

 

熔敷金属力学性能 Mechanical properties of weld metal:

Chinhu chekuyedza

Simba rekusimba

Mpa

Simba rekupa

Mpa

Kureba

%

Kukosha kwemhedzisiro (J)

-30℃

Yakavimbiswa

≥540

≥440

≥17

≥27

Kuongorora X-ray: Giredhi rechipiri

 

Inokurudzirwa yemagetsi:

(mm)

Dhayamita yetsvimbo

2.5

3.2

4.0

5.0

(A)

Welding Current

40 ~ 70

70 ~ 110

110 ~ 160

160 ~ 190

 

Cherechedza:

1. Bvisa tsvimbo yekunamira usati washandisa, woishandisa zvakanyanya kana wapedza kuibvisa;

2. Kazhinji, hapana chikonzero chekuomesa zvakare usati wabatanidza, uye inogona kuomeswa pa70~90°C kweawa imwe chete kana yanyorova.

 

Wenzhou Tianyu Electronic Co., Ltd. yakavambwa muna 2000. Tave tichiita basa rekugadziraelectrode yekunamiras, tsvimbo dzekunamira, uye zvinoshandiswa pakusonwa kwemidziyo kwemakore anopfuura makumi maviri.

Zvigadzirwa zvedu zvikuru zvinosanganisira simbi isina nguraelectrode yekunamiras, maelectrode ekuwedera esimbi yekabhoni,maerekitirodhi ekuwedhesa esimbi akaderera, maelectrode ekuwelda pamusoro, maelectrode ekuwelda enickel & cobalt alloy, waya dzekuwelda dzesimbi dzakapfava & dzakaderera, waya dzekuwelda dzesimbi isingatsvi, waya dzakavharirwa negesi, waya dzekuwelda dzearuminiyamu, welding yearuminiyamu yakanyungudutswa. waya, waya dzekuwelda dzenickel & cobalt alloy, waya dzekuwelda dzebrass, waya dzekuwelda dzeTIG & MIG, maelectrode etungsten, maelectrode ekugocha kabhoni, nezvimwe zvinhu zvekuwelda & zvinodyiwa.

 


  • Yakapfuura:
  • Zvinotevera: