Magadzirirwo ehunyanzvi uye mashandisirwo eStainless Steel Welding Electrodes

Kusonwa kwesimbi isina ngurainzira yakakosha mukugadzirwa kwemazuva ano, inoda zvinhu zvinoshandiswa zvinovimbisa kuramba ngura uye kuvimbika kwechimiro. Iyo electrode yeE308-16 chishandiso chakakosha chakagadzirirwa chinangwa ichi. Se electrode yakagadzirwa netitanium-type coated, yakagadzirwa kuti ishandiswe nesimbi dzisina ngura dzakanyanya kuderera, ichiumba chikamu chakakosha chemaitiro mazhinji ekugadzirisa nekugadzira maindasitiri. Kuvimbika kwechimiro chose chakasungirirwa kunowanzoenderana nesarudzo chaiyo yema electrode akadaro akasarudzika, zvichiita kuti kunzwisisa kwehunhu hwavo kuve kwakakosha kune vanobatanidza ma welding nemainjiniya.

 

E308-16 electrode yakagadzirwa nemakemikari kuti ishandiswe mukubatanidza simbi isina ngura: kubatanidza 18% chromium uye 8% nickel steels. Musanganiswa uyu ndeimwe yemhando dzakajairika dze austenitic, uye makemikari e electrode akanyatsoenzaniswa kuti aenderane nekudzivirira kwayo ngura uye hunhu hwemakanika. Zita rekuti "L" musimbi yayo inoenderana rinoratidza huwandu hwakaderera hwekabhoni, izvo zvakakosha pakudzivirira kunaya kwe carbide panguva yekusanganisa. Izvi zvinoita kuti jointi yakasungirirwa irambe ichidzivirira ngura pakati pe granular, nzvimbo inowanzo kundikana musimbi isina ngura isina ngura.

 

Kushandiswa kwe electrode iyi mukusona simbi isina ngurayakakura, kunyanya muindasitiri. Yakakodzera zvikuru kugadzira zvivakwa zvakagadzirwa nesimbi isingatsvedzeri ye022Cr19Ni10 (yakajairika muChinese standard grade yakaenzana ne304L). Inoshandiswa zvakanyanya mukugadzira michina yenzvimbo dzakaoma, mafekitori ekugadzira mafiber, nzvimbo dzekugadzira fetereza uye michina yakasiyana-siyana yepetrochemical. Mukushandiswa uku, kusimba kweweld kunopihwa neE308-16 kwakakosha pakudzivirira ngura uye kuchengetedza kuchengetedzeka kwekushanda.

 

Hunhu hwekushanda kweE308-16 hunoita kuti ive sarudzo inoshanduka-shanduka yenzvimbo dzakasiyana dzekunamira. Chidimbu che "-16″ muchikamu chayo chinoratidza kuti ine chifukidziro che lime-titania, chinotsigira kunamira munzvimbo dzese.—yakati sandara, yakatwasuka, yakatwasuka, uye yepamusoro. Iyi ibhenefiti huru mukugadzira nekugadzikisa munda uko kugadzirisa zvikamu kusingashande. Arc yakagadzikana, slag inobviswa nyore nyore, uye chitarisiko chebead chakatsetseka, izvo zvinobatsira pamwe chete mukuita basa repamusoro-soro rekuwelda simbi isina ngura uye inoshanda zvakanaka pasina kuchenesa kwakanyanya mushure mekuwelda.

 

E308-16 electrode yakagadzirwa nemazvo inotarisa matambudziko chaiwo ekushandisa.kusona simbi isina ngurapamhando dzakaderera dzekabhoni. Kushandiswa kwayo kwemakemikari kwakatarwa pasimbi 18-8 uye kukodzera kwayo kumaindasitiri akakosha akadai semafuta nefetereza zvinosimbisa kukosha kwayo. Kune nyanzvi dzinoshanda mukusanganisa simbi isingatsvedzi, kusarudza electrode yeE308-16 yemapurojekiti akakodzera kunopa nzira yakavimbika yekuwana ma weld akasimba, anodzivirira ngura anosangana nezvinodiwa zvakasimba zvekushanda uye kuchengetedzeka mumashandisirwo emaindasitiri.

Kushongedza Simbi Isina Kusimba


Nguva yekutumira: Mbudzi-25-2025