Electrode yeAluminium Alloy yemhando yepamusoro E4043

Aruminiyamu neAruminiyamu Chiwanikwa ElectrodeAWS E4043

Tsananguro: AWS E4043 ielectrode yealuminium-silicon alloy ine coating inobva mumunyu. Shandisa DCEP (direct current electrode positive). Short arc fast test welding. Simbi yakachengetwa ine simba remakanika uye inodzivirira kutsemuka zvakanaka. 

Mashandisirwo: . Inoshandiswa pakusanganisa plate yearuminiyamu, kusanganisa aruminiyamu nesilicon, general alloy yearuminiyamu, aruminiyamu yakagadzirwa uye duralumin. Asi haina kukodzera pakusanganisa aruminiyamu nemagnesium.

Kuumbwa kwemakemikari esimbi ye weld (%):

Si

Fe

Cu

Mn

Ti

Zn

Al

Mg

Zvimwe

4.5 ~ 6.0

≤0.8

≤0.30

≤0.05

≤0.20

≤0.10

Ramba uripo

≤0.05

≤0.15

 

Inokurudzirwa yemagetsi:

Dhayamita yetsvimbo (mm)

3.2

4.0

5.0

Kukweshera Kwemazuva (A)

80 ~ 100

110 ~ 150

150 ~ 200

 

 Cherechedza:

1. Electrode iri nyore kukanganiswa nehunyoro, saka inofanira kuchengetwa mumudziyo wakaoma usingapindi mhepo kuti isaora nekuda kwehunyoro; electrode inofanira kubikwa pa150°C kweawa imwe kusvika maviri isati yaiswa welding;

2. Maplate ekumashure anofanira kushandiswa usati wabatanidza, uye kusanganisa kunofanira kuitwa mushure mekudziya kusvika 200 ~ 300°C zvichienderana neukobvu hwekubatanidza; tsvimbo yekusanganisa inofanira kunge yakatarisana nepamusoro pekubatanidza, arc inofanira kunge iri pfupi sezvinobvira, uye kutsiva tsvimbo dzekusanganisa kunofanira kuitwa nekukurumidza;

3. Kubatanidza kunofanira kucheneswa kubva mumafuta netsvina isati yabatanidzwa, uye tsvina inofanira kubviswa nokungwarira mushure mekusanganisa, uye kusukurudzwa neutsi kana mvura inopisa.

 

E4043png