Uri Kushandisa Tsvimbo Dzakakodzera Here?

Vazhinji vanopinza tambo dzemagetsi vanowanzo dzidza nerudzi rumwe chete rweelectrode. Zvine musoro. Zvinokutendera kuti ugadzirise hunyanzvi hwako pasina kunetseka nezvema parameters nema settings akasiyana. Ndiyo zvakare inokonzera dambudziko guru pakati pevanopinza tambo dzemagetsi vanobata mhando dzese dzeelectrode zvakafanana. Kuti uve nechokwadi chekuti hauzombowirwi, takaunganidza gwara rakakwana remhando dzeelectrode uye mashandisirwo adzo.

E6010

Zvese 6010 na6011 itsvimbo dzeFast Freeze. Fast Freeze zvinoreva chaizvo zvaunofunga (ndatenda shamwari yewelding). Maelectrode eFast Freeze anotonhora nekukurumidza kupfuura mamwe marudzi, zvichiita kuti dziva risaputike uye ripise zvakanyanya. Izvi zvinoreva kuti unokwanisa kuisa pasi bead rakatetepa rinopinda zvakanyanya mu workpiece yako. Rinokutendera kuti upise nengura uye zvinhu zvakasviba, saka haufanirwe kuchenesa zvinhu zvako usati waisa welding. Chinhu chimwe chekurangarira ndechekuti 6010 rods dzinoshanda chete paDirect Current Electrode Positive.

E6011

Maerekitironi anogadzirwa, haasi ekuzvarwa. Asi dai akagadzirwa, 6011 yaizova hanzvadzi yemapatya ye6010. Ose ari maviri maFast Freeze rods, zvichiita kuti ave akanaka pamidzi uye pakubatanidza mapaipi. Dziva ravo diki rekubatanidza rinosiya tsvina shoma kuti rive nyore kuchenesa. Kunyange zvazvo 6011 yakagadzirirwa michina yeAC, inogonawo kushanda paDC ichipa mukana pamusoro pe6010 electrodes (iyo inogona chete kuita Direct Current Electrode Positive).

E6013

Chikanganiso chinowanzoitwa nevaStick welders ndechekugadzirisa maelectrode avo e6013 akadai se6011 kana 6010 rods. Kunyange zvazvo yakafanana mune zvimwe zvinhu, 6013 ine slag yesimbi inoda simba rakawanda kuti ipfuure. VaWelders vanovhiringidzika kana mabheya avo azere nemaburi ehonye, ​​​​vasingazive kuti vanofanira kukwidza maamps avo. Uchazvidzivirira pamatambudziko akawanda nekungotarisa marongero aunoda usati watanga kushandisa rudzi rutsva rwetsvimbo. Zviri nyore, kunyanya neimwe yemapurogiramu edu ewelding emahara atinofarira (aunogona kuwana pano). Zvakakoshawo kuchenesa simbi yako zvakanyanya sezvinobvira usati watanga welding. 6013 ine kupinda kwakapfava nedziva guru risingapfuure ngura se6010 kana 6011.

E7018

Electrode iyi inonyanya kufarirwa nevanogadzira machira zvichibva paarc yayo yakatsetseka. Kupinda kwayo zvinyoro nyoro uye dziva guru zvinosiya mabhora makuru, akasimba, asina kunyatsojeka. Kufanana ne6013, kupinda kwayo zvinyoro nyoro zvinoreva kuti unofanira kuva nenzvimbo dzakachena dzekupinza. Saizvozvowo, ma7018 ane maparamita akasiyana nedzimwe tsvimbo saka ita shuwa kuti waongorora marongero ako usati watanga.

Kune nyanzvi zhinji, chinhu chakanyanya kuoma nezvemaerekitirodhi aya kuachengeta zvakanaka. Kana bhokisi ravhurwa, zvakanaka kuchengeta maerekitirodhi asara muovheni yerodhi. Pfungwa ndeyekudzivirira hunyoro kuti husapinde mumhepo nekuachengeta achipisa pa250 degrees.

E7024

Iyo 7024 ndiyo hombe yema electrodes, ine jira rinorema uye rinorema re slag coating. Kufanana ne7018, inosiya bead rakanaka, rakatsetseka rine kupinda kwakapfava uye rinoda nzvimbo yakachena kuti ishande. Pane matambudziko maviri akajairika ayo nyanzvi dzinowanzoona ne 7024 rods. Chekutanga, vanowelda havashandisi simba re arc rakakwana kusunda slag uye vanopedzisira vaine weld inoshivirira, kunyange isina kukwana. Zvakare, masekondi mashanu anokurumidza paapp ye reference guide achakununura matambudziko akawanda. Dambudziko rimwe nderekuti kana vanowelda vachiedza kushandisa 7024 rods pa overhead welds. Slag inorema inoshanduka kuita mabhora emoto anonaya zvichireva kuti hauzodi kugerwa nebvudzi kwenguva yakati.

Ehe, kushandisa tsvimbo dzakakodzera hazvina basa kana dzichibva kumhando dzisina kujairika. Nerombo rakanaka tinotsigira zvese zvatinoshandisa kuti tikupei welds dzakanakisisa. Tarisa mutsauko unogona kukonzerwa netambo dzemuchitoro chikuru pano.